A Preliminary Study on the Detection Methods of Stress and Strain in the Process of Wood Drying. In the process of wood drying, both elastic stress and residual stress affect the drying quality; after the drying process is completed and the moisture content distribution across the thickness of the wood becomes uniform, the elastic strain has disappeared, and it is residual stress that continues to affect the drying quality thereafter.
1. Stress and Deformation Caused by Inconsistent Tangential and Radial Shrinkage of Wood
Based on the characteristic that the tangential shrinkage coefficient of wood is approximately twice that of the radial shrinkage coefficient, this paper analyzes the shrinkage, stress and deformation of three types of wood. a. Radially cut boards: all board surfaces are radial cut surfaces, and the entire board thickness is in the tangential direction. The shrinkage is uniform, so no additional stress and deformation will be caused. b. Tangentially cut boards: the outer board surface (the surface close to the bark) is close to the tangential direction, and its shrinkage amount is larger than that of the inner board surface (the surface close to the pith) which is close to the radial direction. Therefore, the board will warp toward the outer board surface during drying. However, in actual drying production, boards are stacked into a wood pile, and weight blocks are placed on the top of the pile to prevent wood warping and deformation. Due to the weight of the wood pile and the weight blocks, additional pressure is generated on the boards to restrain their warping. As a result, additional tensile stress is generated on the outer board surface of the board, and additional compressive stress is generated on the inner board surface. This stress has nothing to do with the moisture content gradient. The additional tensile stress on the outer board surface superimposes with the surface tensile stress caused by uneven moisture content, which can easily cause surface cracking on the outer board surface. c. Square timber with pith: its four surfaces are close to tangential cut surfaces, and their shrinkage amount is larger than that in the diameter direction. During drying, the shrinkage of the four surfaces is restrained by the wood in the internal diameter direction. As a result, additional tensile stress is generated in the surface layer area, and additional compressive stress is generated in the central area. This stress also has nothing to do with the moisture content gradient. This additional surface tensile stress superimposes with the tensile stress caused by the moisture content gradient in the early drying stage, which can easily cause surface cracking and radial cracking. Therefore, square timber with pith is very prone to produce defects during drying. Stress and deformation caused by uneven moisture content across the thickness of wood.